Hoyte Designs Twynzer for Orlo

This was a fun, but challenging board!

Let me explain...

Blank: EPS = open celled foam which needs to be sealed and then sanded back before the glassing to prevent blowing air.
 



Now add a concave, curve channel which, even on 'clears', is hard to get even and bubble-less.




If seen up close, one can see a near flawless cut lap on the deck from the bottom lamination.

No pinline required here.



The challenging part was keeping the tint even over a porous surface and to tape of the lams without pulling foam beads out.



Final product = near perfection.

Orlo is stoked! :)